Nicola M Everitt
Nanoindentation shows uniform local mechanical properties across melt pools and layers produced by selective laser melting of AlSi10Mg alloy
Everitt, Nicola M; Aboulkhair, Nesma T.; Maskery, Ian; Tuck, Christopher; Ashcroft, Ian
Authors
Nesma T. Aboulkhair
Dr IAN MASKERY IAN.MASKERY@NOTTINGHAM.AC.UK
Assistant Professor
CHRISTOPHER TUCK CHRISTOPHER.TUCK@NOTTINGHAM.AC.UK
Professor of Materials Engineering
IAN ASHCROFT IAN.ASHCROFT@NOTTINGHAM.AC.UK
Professor of Mechanics of Solids
Abstract
Single track and single layer AlSi10Mg has been produced by selective laser melting (SLM) of alloy powder on a AlSi12 cast substrate. The SLM technique produced a cellular-dendritic ultra-fined grained microstructure. Chemical composition mapping and nanoindentation showed higher hardness in the SLM material compared to its cast counterpart. Importantly, although there was some increase of grain size at the edge of melt pools, nanoindentation showed that the hardness (i.e. yield strength) of the material was uniform across overlapping tracks. This is attributed to the very fine grain size and homogeneous distribution of Si throughout the SLM material.
Journal Article Type | Article |
---|---|
Acceptance Date | Dec 5, 2015 |
Publication Date | Jan 12, 2016 |
Deposit Date | Jul 25, 2016 |
Publicly Available Date | Jul 25, 2016 |
Journal | Advanced Materials Letters |
Electronic ISSN | 0976-3961 |
Peer Reviewed | Peer Reviewed |
Volume | 7 |
Issue | 1 |
DOI | https://doi.org/10.5185/amlett.2016.6171 |
Keywords | Nanoindentation; additive manufacturing; aluminium alloy |
Public URL | https://nottingham-repository.worktribe.com/output/772957 |
Publisher URL | https://www.researchgate.net/publication/289229850_Nanoindentation_shows_uniform_local_mechanical_properties_across_melt_pools_and_layers_produced_by_selective_laser_melting_of_AlSi_10Mg_alloy |
Files
ADvmatlettNME2015_final.pdf
(413 Kb)
PDF
Copyright Statement
Copyright information regarding this work can be found at the following address: http://creativecommons.org/licenses/by/4.0
You might also like
Functionalized Gold Nanoparticles with a Cohesion Enhancer for Robust Flexible Electrodes
(2022)
Journal Article
Stochastic design for additive manufacture of true biomimetic populations
(2022)
Journal Article
Downloadable Citations
About Repository@Nottingham
Administrator e-mail: discovery-access-systems@nottingham.ac.uk
This application uses the following open-source libraries:
SheetJS Community Edition
Apache License Version 2.0 (http://www.apache.org/licenses/)
PDF.js
Apache License Version 2.0 (http://www.apache.org/licenses/)
Font Awesome
SIL OFL 1.1 (http://scripts.sil.org/OFL)
MIT License (http://opensource.org/licenses/mit-license.html)
CC BY 3.0 ( http://creativecommons.org/licenses/by/3.0/)
Powered by Worktribe © 2024
Advanced Search