Abstract
High velocity oxy-fuel thermal spraying was used to prepare free-standing CoNiCrAlY (Co–31.7% Ni–20.8% Cr–8.1% Al–0.5% Y (wt%)) bond coat alloy samples approximately 0.5 mm thick. Creep tests were conducted at 750 °C on these samples using a small punch (SP) creep test method. The samples were characterised before and after creep testing using scanning electron microscopy with electron backscatter diffraction (EBSD). EBSD revealed a two phase fcc γ-Ni and bcc B2 β-NiAl microstructure with grain sizes ~1–2 μm for both phases, which did not change significantly following testing. The constant temperature SP test data were characterised by a minimum creep strain rate, View the MathML source, and a total time to failure, tf, at different applied stresses. The data are fitted to conventional power law equations with a stress exponent for creep close to 8 in the Norton power law and between 7 and 10 in the Monkman–Grant creep rupture law. Creep rupture was predominantly due to creep cavitation voids nucleating at both the γ–β interphase boundaries and the γ–γ grain boundaries leading to final failure by void linkage. However, rupture life was influenced by the quantity of oxide entrained in the coating during the spray deposition process.
Journal Article Type | Article |
---|---|
Publication Date | Jan 1, 2013 |
Deposit Date | Jul 23, 2014 |
Publicly Available Date | Jul 23, 2014 |
Journal | Materials Science and Engineering: A |
Print ISSN | 0921-5093 |
Electronic ISSN | 0921-5093 |
Publisher | Elsevier |
Peer Reviewed | Peer Reviewed |
Volume | 585 |
DOI | https://doi.org/10.1016/j.msea.2013.06.080 |
Keywords | HVOF thermal spraying; MCrAlY bond coat; Mechanical testing; Creep; Phase transformation |
Public URL | https://nottingham-repository.worktribe.com/output/1003651 |
Publisher URL | http://www.sciencedirect.com/science/article/pii/S0921509313007429 |
Additional Information | NOTICE: this is the author’s version of a work that was accepted for publication in Materials Science and Engineering: A. Changes resulting from the publishing process, such as peer review, editing, corrections, structural formatting, and other quality control mechanisms may not be reflected in this document. Changes may have been made to this work since it was submitted for publication. A definitive version was subsequently published in Materials Science and Engineering: A, 585 (2013), doi: 10.1016/j.msea.2013.06.080 |
Files
Unformatted_MSEA-S-13-00981erep.pdf
(2.3 Mb)
PDF
You might also like
Image processing algorithm to determine an optimised 2D laser cutting trajectory
(2019)
Conference Proceeding
Establishing Optimal Parameters For Laser Cutting Of Thin Semitransparent Organic Material
(2019)
Presentation / Conference
Corrosion inhibition of mild steel in 15 wt.% HCl by durum wheat
(2017)
Conference Proceeding
Downloadable Citations
About Repository@Nottingham
Administrator e-mail: discovery-access-systems@nottingham.ac.uk
This application uses the following open-source libraries:
SheetJS Community Edition
Apache License Version 2.0 (http://www.apache.org/licenses/)
PDF.js
Apache License Version 2.0 (http://www.apache.org/licenses/)
Font Awesome
SIL OFL 1.1 (http://scripts.sil.org/OFL)
MIT License (http://opensource.org/licenses/mit-license.html)
CC BY 3.0 ( http://creativecommons.org/licenses/by/3.0/)
Powered by Worktribe © 2024
Advanced Search