Numerical Investigation into the Influence of Grain Orientation Distribution on the Local and Global Elastic-Plastic Behaviour of Polycrystalline Nickel-Based Superalloy INC-738 LC
Engel, Benedikt; Huth, Mark; Hyde, Christopher
Abstract
Polycrystalline nickel-based superalloys tend to have large grains within component areas where high loads are dominant during operation. Due to these large grains, caused by the manufacturing and cooling process, the orientation of each grain becomes highly important, since it influences the elastic and plastic behaviour of the material. With the usage of the open source codes NEPER and FEPX, polycrystalline models of Inconel 738 LC were generated and their elastic and crystal plasticity behaviour simulated in dependence of different orientation distributions under uniaxial loading. Orientation distributions close to the [100] direction showed the lowest Young’s moduli as well as the highest elastic strains before yielding, as expected. Orientations close to the [589] direction, showed the lowest elastic strains and therefore first plastic deformation under strain loading due to the highest shear stress in the slip systems caused by the interaction of Young’s modulus and the Schmid factor.
Citation
Engel, B., Huth, M., & Hyde, C. (2022). Numerical Investigation into the Influence of Grain Orientation Distribution on the Local and Global Elastic-Plastic Behaviour of Polycrystalline Nickel-Based Superalloy INC-738 LC. Crystals, 12(1), Article 100. https://doi.org/10.3390/cryst12010100
Journal Article Type | Article |
---|---|
Acceptance Date | Jan 11, 2022 |
Online Publication Date | Jan 13, 2022 |
Publication Date | Jan 13, 2022 |
Deposit Date | Mar 23, 2022 |
Publicly Available Date | Mar 23, 2022 |
Journal | Crystals |
Electronic ISSN | 2073-4352 |
Publisher | MDPI |
Peer Reviewed | Peer Reviewed |
Volume | 12 |
Issue | 1 |
Article Number | 100 |
DOI | https://doi.org/10.3390/cryst12010100 |
Public URL | https://nottingham-repository.worktribe.com/output/7345790 |
Publisher URL | https://www.mdpi.com/2073-4352/12/1/100 |
Files
Numerical Investigation into the Influence of Grain Orientation Distribution on the Local and Global Elastic-Plastic Behaviour of Polycrystalline Nickel-Based Superalloy INC-738 LC
(1.7 Mb)
PDF
Publisher Licence URL
https://creativecommons.org/licenses/by/4.0/
You might also like
The Estimation of Taylor-Quinney Coefficients Using Small Ring Specimens
(2022)
Journal Article
MHT ECCC 2021 special issue introduction
(2022)
Journal Article
Downloadable Citations
About Repository@Nottingham
Administrator e-mail: discovery-access-systems@nottingham.ac.uk
This application uses the following open-source libraries:
SheetJS Community Edition
Apache License Version 2.0 (http://www.apache.org/licenses/)
PDF.js
Apache License Version 2.0 (http://www.apache.org/licenses/)
Font Awesome
SIL OFL 1.1 (http://scripts.sil.org/OFL)
MIT License (http://opensource.org/licenses/mit-license.html)
CC BY 3.0 ( http://creativecommons.org/licenses/by/3.0/)
Powered by Worktribe © 2025
Advanced Search