Abstract
© 2020 The Authors While laser-assisted machining can significantly improve the machinability of nickel-based superalloy, the mechanism of surface integrity evolution and its influence on the material functional performance is still not clear. The present study gives a comprehensive investigation on the surface integrity of laser-assisted milling (LAMill) process with an in-depth study of the mechanism of chip formation, microstructural and mechanical alternations, supported by key outcomes from the two constitutive processes, conventional milling (CMill) and single laser scanning (LS). Although the high thermal affected layer in LAMill process has been removed through the cutting chips, a significant bending effect has been found in both the LAMill and LS workpiece. More interestingly, a combined impact of the residual stress from LS and CMill has been found on LAMill workpiece while a lattice evolution has been revealed regarding both the thermal and mechanical influence. Specifically, inadequate fatigue performance on LAMill and LS workpiece has been found due to the high thermal effect in the superficial layer regarding the residual tensile stress distribution and microstructure variation. While LAMill is generally considered as a promising machining method with improved machinability of difficult-to-cut materials, this research shows a poor workpiece functional performance (fatigue) and justifies its application prospect.
Citation
Xu, D., Liao, Z., Axinte, D., Sarasua, J. A., M'Saoubi, R., & Wretland, A. (2020). Investigation of surface integrity in laser-assisted machining of nickel based superalloy. Materials and Design, 194, Article 108851. https://doi.org/10.1016/j.matdes.2020.108851
Journal Article Type | Article |
---|---|
Acceptance Date | Jun 2, 2020 |
Online Publication Date | Jun 5, 2020 |
Publication Date | Sep 1, 2020 |
Deposit Date | Jun 6, 2020 |
Publicly Available Date | Jun 8, 2020 |
Journal | Materials and Design |
Print ISSN | 0264-1275 |
Electronic ISSN | 1873-4197 |
Publisher | Elsevier |
Peer Reviewed | Peer Reviewed |
Volume | 194 |
Article Number | 108851 |
DOI | https://doi.org/10.1016/j.matdes.2020.108851 |
Keywords | Mechanical Engineering; General Materials Science; Mechanics of Materials |
Public URL | https://nottingham-repository.worktribe.com/output/4597263 |
Publisher URL | https://www.sciencedirect.com/science/article/pii/S0264127520303853 |
Files
1-s2.0-S0264127520303853-main
(6.9 Mb)
PDF
Publisher Licence URL
https://creativecommons.org/licenses/by-nc-nd/4.0/
You might also like
Multimodal locomotion ultra-thin soft robots for exploration of narrow spaces
(2024)
Journal Article
Modelling of modular soft robots: From a single to multiple building blocks
(2024)
Journal Article
Downloadable Citations
About Repository@Nottingham
Administrator e-mail: discovery-access-systems@nottingham.ac.uk
This application uses the following open-source libraries:
SheetJS Community Edition
Apache License Version 2.0 (http://www.apache.org/licenses/)
PDF.js
Apache License Version 2.0 (http://www.apache.org/licenses/)
Font Awesome
SIL OFL 1.1 (http://scripts.sil.org/OFL)
MIT License (http://opensource.org/licenses/mit-license.html)
CC BY 3.0 ( http://creativecommons.org/licenses/by/3.0/)
Powered by Worktribe © 2025
Advanced Search